Product Details
Main function and features
Separation Plate
Ore |
Particle size distribution |
Feeding concentration |
Treatment capacity kg(m2h)-1 |
Filter cake moisture |
Gold concentrate |
-200~-325 meshes |
50~60 |
900~1500 |
6.5~11.5 |
Gold tailing |
-200~-400 meshes |
50~60 |
400~600 |
13~16 |
Copper concentrate |
-200~-325 meshes |
50~60 |
600~900 |
6.5~12 |
Iron concentrate |
-200~-325 meshes |
50~60 |
850~1500 |
6~10 |
Zinc concentrate |
-200~-400 meshes |
50~60 |
750~900 |
6.5~12 |
Lead concentrate |
-200~-325 meshes |
50~60 |
650~800 |
10~12 |
Aluminum concentrate |
-200~-325 meshes |
50~60 |
350~450 |
10.5~12 |
Lead-zinc tailing |
-200~-325 meshes |
50~65 |
350~550 |
12~16 |
Cyanide residue |
-200~-450 meshes |
50~60 |
350~550 |
21~24 |
Sulfur concentrate |
-200 meshes 80% |
50~65 |
350~790 |
8~12 |
Nickel concentrate |
-200~-325 meshes |
55~60 |
300~600 |
10~12 |
Clean coal |
--200 meshes (accounting for 80%) |
50~65 |
550~930 |
18~20 |
Zinc oxide |
-200 meshes (accounting for 75%) |
55~65 |
620~1200 |
8~12 |
Fluorescent powder |
-200 meshes (accounting for 60%) |
55~65 |
750~900 |
8~12 |